Sign In | Join Free | My himfr.com |
|
Ask Lasest Price | |
Brand Name : | High Broad or OEM |
Model Number : | AZ31B |
Certification : | ISO, DNV,BV |
Price : | negotiable |
Payment Terms : | L/C, D/A, D/P, T/T, Western Union, MoneyGram,Paypal |
Supply Ability : | 500mt/month |
Delivery Time : | 1FCL: 14 days |
Extrude Cast Aluminium vs Magnesium Anode Rod In Hot Water Systems , electric water heater
High Broad provides extruded magnesium anodes and aluminum anodes in various sizes with welded steel caps / resistor fittings for commercial water heaters.
Magnesium anodes are available with grade M-1/ AZ31 alloys with diameter sizes ranging between 0.50 to 1.05 inches. All products are produced under ISO standards, with quality tested by High Broad on a regular basis
Magnesium sacrificial anode protects against galvanic corrosion and extends the life of the water heater.
Suits all Kuuma and Force 10 brand marine water heaters.
Part Number: 41919A
Anode Material: Magnesium
Thread: 3/4" - 14 NPT
Total Length: 130mm / 5.1"
Other anodes you may have interests:
Water Heater Mg/Al/Zn Anode Rods
Aluminum Anodes for Hull, Pier,Piling,Deck
Zinc anodes for Ship, Marine
Zinc Ribbon anodes
Magnesium Anodes for underground pipelines,tanks
Magnesium material for cell application
Contact me for more details :
Vivian Jiang
International Marketing & Sales Department Manager
-----------------------------------------------
China Hunan High Broad New Material Co.Ltd.
70 Chezhan North Road,Changsha, China 410100
Tel:+86-731-85717705 Fax:+86-731-85716569
Mobile/Whatsapp: +86-139-7488-3816
Email: vivian@hbnewmaterial.com , metal@vip.163.com
Sacrificial anodes are usually made from relatively pure active metals, such as magnesium, aluminum, or zinc. These more active metals (anodes) oxidize and corrode much faster than the less active metals (cathodes).
Magnesium generates around -1.6 volts
Aluminum generates around -1.1 volts
Zinc generates around -1.05 volts
As a result, magnesium anode rods tend to work better (succumbs to corrosion faster), but don’t last as long as other metals.
The anode rod is “self-sacrificing” and will continue to corrode until eventually it must be replaced. When there’s no sacrificial metal left on the anode, the tank can rust out, eventually causing it to burst.
![]() |